%0 Journal Article %T Investigation of Barium Sulfate Precipitation and Prevention Using Different Scale Inhibitors under Reservoir Conditions %J International Journal of Engineering %I Materials and Energy Research Center %Z 1025-2495 %A Khormali, A. %A Sharifov, A. R. %A Torba, D. I. %D 2018 %\ 10/01/2018 %V 31 %N 10 %P 1796-1802 %! Investigation of Barium Sulfate Precipitation and Prevention Using Different Scale Inhibitors under Reservoir Conditions %K barium sulfate %K Formation Damage %K Scale Inhibition %K Scale Prediction %R %X In this work, scaling tendency and amount of precipitation of barium sulfate (BaSO4) were determined; the process is depending on temperature, pressure and mixing ratio of injection and formation of waters. Results showed that BaSO4 precipitation is largely dependent on mixing ratio. Temperature and pressure had no influence on BaSO4 precipitation. Different scale inhibitors, including a new inhibitor package, were used for preventing BaSO4 precipitation. The new scale inhibitor consists of three different acids such as phosphonate acid, hydrochloric acid solution, isopropyl alcohol, ammonium chloride and water. In addition, the lowest interfacial tensionon the boundary of oil and new inhibitor occurred at 10% of hydrochloric acid. Furthermore, effect of temperature, mixing ratio of waters and barium concentration on the inhibition efficiency of BaSO4 formation was studied. Results showed that the new inhibitor has the highest efficiency for preventing BaSO4 precipitation at any temperature, mixing ratio and barium concentration. Moreover, formation damage due to BaSO4 formation with and without scale inhibitors was determined by core flood tests. In the presence of new inhibitor, the damaged rock permeability ratio was improved from 0.59 to 0.924. %U https://www.ije.ir/article_82223_abe367b0cabb4fd905d8d1372c39e0a5.pdf